@article{MiyamatoSakakitaWagneretal.2015, author = {Miyamato, Ko-ichiro and Sakakita, Sakura and Wagner, Torsten and Sch{\"o}ning, Michael Josef and Yoshinobu, Tatsuo}, title = {Application of chemical imaging sensor to in-situ pH imaging in the vicinity of a corroding metal surface}, series = {Electrochimica Acta}, volume = {183}, journal = {Electrochimica Acta}, publisher = {Elsevier}, address = {Amsterdam}, issn = {0013-4686}, doi = {10.1016/j.electacta.2015.07.184}, pages = {137 -- 142}, year = {2015}, abstract = {The chemical imaging sensor was applied to in-situ pH imaging of the solution in the vicinity of a corroding surface of stainless steel under potentiostatic polarization. A test piece of polished stainless steel was placed on the sensing surface leaving a narrow gap filled with artificial seawater and the stainless steel was corroded under polarization. The pH images obtained during polarization showed correspondence between the region of lower pH and the site of corrosion. It was also found that the pH value in the gap became as low as 2 by polarization, which triggered corrosion.}, language = {en} } @article{SchusserPoghossianBaeckeretal.2015, author = {Schusser, Sebastian and Poghossian, Arshak and B{\"a}cker, Matthias and Krischer, M. and Leinhos, Marcel and Wagner, P. and Sch{\"o}ning, Michael Josef}, title = {An application of field-effect sensors for in-situ monitoring of degradation of biopolymers}, series = {Sensors and actuators B: Chemical}, volume = {207, Part B}, journal = {Sensors and actuators B: Chemical}, publisher = {Elsevier}, address = {Amsterdam}, issn = {1873-3077 (E-Journal); 0925-4005 (Print)}, doi = {10.1016/j.snb.2014.10.058}, pages = {954 -- 959}, year = {2015}, abstract = {The characterization of the degradation kinetics of biodegradable polymers is mandatory with regard to their proper application. In the present work, polymer-modified electrolyte-insulator-semiconductor (PMEIS) field-effect sensors have been applied for in-situ monitoring of the pH-dependent degradation kinetics of the commercially available biopolymer poly(d,l-lactic acid) (PDLLA) in buffer solutions from pH 3 to pH 13. PDLLA films of 500 nm thickness were deposited on the surface of an Al-p-Si-SiO2-Ta2O5 structure from a polymer solution by means of spin-coating method. The PMEIS sensor is, in principle, capable to detect any changes in bulk, surface and interface properties of the polymer induced by degradation processes. A faster degradation has been observed for PDLLA films exposed to alkaline solutions (pH 9, pH 11 and pH 13).}, language = {en} }