Refine
Year of publication
Institute
Has Fulltext
- no (87) (remove)
Document Type
- Conference Proceeding (41)
- Article (37)
- Part of a Book (4)
- Report (2)
- Book (1)
- Contribution to a Periodical (1)
- Patent (1)
Is part of the Bibliography
- no (87)
Application of polymers in textile reinforced concrete : from the interface to construction elements
(2006)
Composite improvement of textile reinforced concrete by polymeric impregnation of the textiles
(2006)
Mikrokleben
(2005)
In this research work, a statistical analysis of the CO2 laser beam welding of dual phase (DP600)/transformation induced plasticity (TRIP700) steel sheets was done using response surface methodology. The analysis considered the effect of laser power (2–2.2 kW), welding speed (40–50 mm/s) and focus position (−1 to 0 mm) on the heat input, the weld bead geometry, uniaxial tensile strength, formability limited dome height and welding operation cost. The experimental design was based on Box–Behnken design using linear and quadratic polynomial equations for predicting the mathematical models. The results indicate that the proposed models predict the responses adequately within the limits of welding parameters being used and the welding speed is the most significant parameter during the welding process.
Generally, the quality of a weld joint is directly influenced by the welding input parameter settings. Selection of proper process parameters is important to obtain the desired weld bead profile and quality. In this research work, numerical and graphical optimization techniques of the CO2 laser beam welding of dual phase (DP600)/transformation induced plasticity (TRIP700) steel sheets were carried out using response surface methodology (RSM) based on Box–Behnken design. The procedure was established to improve the weld quality, increase the productivity and minimize the total operation cost by considering the welding parameters range of laser power (2–2.2 kW), welding speed (40–50 mm/s) and focus position (−1 to 0 mm). It was found that, RSM can be considered as a powerful tool in experimental welding optimization, even when the experimenter does not have a model for the process. Strong, efficient and low cost weld joints could be achieved using the optimum welding conditions.
Für Auftragschweißaufgaben existiert eine Vielzahl an verfahrenstechnischen
Prozessvarianten, die je nach Charakteristik und Anwendungsfall
ausgewählt werden. Ein Nachteil der vorwiegend verwendeten Metall-
Schutzgasschweißprozesse (MSG) für das Auftragschweißen ist durch die
direkte Kopplung von Drahtvorschub zu Energieeintrag gegeben. Die vorgestellte
Zweidraht-Prozessvariante kann durch die Ausbildung eines übertragenen
und eines nicht-übertragenen Lichtbogens die elektrische Leistung
beider Lichtbögen variieren und damit einen direkten Einfluss auf
die Prozessgrößen Abschmelzleistung und Aufschmelzgrad nehmen. Im
Speziellen besteht über die Entkopplung von Drahtvorschub zu Schweißstromstärke
die Möglichkeit eines niederenergetischen Betriebs trotz hoher
Drahtvorschubgeschwindigkeit. Damit lassen sich Aufschmelzgrade
unter 2% umsetzen und Abschmelzleistungen bis zu 15 kg/h realisieren.